Quantity: | |
---|---|
1.Rib Lath is also ideal for refurbishing damaged or aged masonry walls when a key for rendering is not certain due to disintegration or softening of the wall face
Widely used as a plaster backing on ceilings, walls and stud partitions.
2.MT Hy rib lath mesh General specifications for your reference:
Thickness mm | Open size(Sw*Lw) mm | Rib height mm | Rib distance mm | Weight Kg/m2 | Width mm |
0.3 | 12×8 | 5 | 100 | 1.2 | 610 |
0.35 | 12×8 | 5 | 100 | 1.4 | 610 |
0.4 | 12×8 | 5 | 100 | 1.6 | 610 |
0.3 | 12×8 | 8 | 100 | 1.2 | 610 |
0.35 | 12×8 | 8 | 100 | 1.4 | 610 |
0.4 | 12×8 | 8 | 100 | 1.6 | 610 |
1.Rib Lath is also ideal for refurbishing damaged or aged masonry walls when a key for rendering is not certain due to disintegration or softening of the wall face
Widely used as a plaster backing on ceilings, walls and stud partitions.
2.MT Hy rib lath mesh General specifications for your reference:
Thickness mm | Open size(Sw*Lw) mm | Rib height mm | Rib distance mm | Weight Kg/m2 | Width mm |
0.3 | 12×8 | 5 | 100 | 1.2 | 610 |
0.35 | 12×8 | 5 | 100 | 1.4 | 610 |
0.4 | 12×8 | 5 | 100 | 1.6 | 610 |
0.3 | 12×8 | 8 | 100 | 1.2 | 610 |
0.35 | 12×8 | 8 | 100 | 1.4 | 610 |
0.4 | 12×8 | 8 | 100 | 1.6 | 610 |